Working brass cold...
-
Presuming this is not a great idea from my 1st failed attempt at making a bale? The ends of a 3mm rod that I am flattening are just becoming brittle and crumbling away. Is it best to heat first before working even though I am use to peening it for pins this seems a step to far for working cold. Same for nickel silver?
Any advice gladly received

-
With cold working, less is more. As tiny taps as possible.
I still think it might be better to heat up to red-hot and allow to cool in air, though.

-
Depends on the temper of the material you’re working with...and how aggressively you are forming it. It does sound like a fairly hard/drawn temper. Anealing should help make it easier to work with. Hard to say without seeing what or how much was done before there were issues.
Reminds me I gotta get some 3mm brass for 111mm modding.
Hello! It looks like you're interested in this conversation, but you don't have an account yet.
Getting fed up of having to scroll through the same posts each visit? When you register for an account, you'll always come back to exactly where you were before, and choose to be notified of new replies (either via email, or push notification). You'll also be able to save bookmarks and upvote posts to show your appreciation to other community members.
With your input, this post could be even better 💗
Register Login