And so it begins.... (My adventures into Alox!)
-
I still build alot of blue tiox super tinkers. This has become quite a standard request. Here the only difference is I removed the keyring from the opener layer spring. Ground off the piece of spring with the hole and then sanded and buffed it. It doenst even look like there ever was one now.




-
Love the color!
JR -
@MadPlumbarian said:
Love the color!
JR+1, the cross really makes it look extra professional. It's nice to see the single piece liner as well, that takes the knife another step above stock configuration.
-
@Syph007 said:
I still build alot of blue tiox super tinkers. This has become quite a standard request. Here the only difference is I removed the keyring from the opener layer spring. Ground off the piece of spring with the hole and then sanded and buffed it. It doenst even look like there ever was one now.



I can see why it's popular! Have you tried doing the Tiox scales in green or purple yet?
-
I still build alot of blue tiox super tinkers. This has become quite a standard request. Here the only difference is I removed the keyring from the opener layer spring. Ground off the piece of spring with the hole and then sanded and buffed it. It doenst even look like there ever was one now.




I can see why it's popular! Have you tried doing the Tiox scales in green or purple yet?
I need to etch the scales to get the higher voltage colors and the best chemical for that is hydrofloric acid. I found a source but havent got any yet.
-
@Ombudsman said:
You can use the Antikythera Mechanism gear template. :D
Do you follow clickspring on youtube, he is starting to do a build of that mechanism.
-
@Syph007 said:
I need to etch the scales to get the higher voltage colors and the best chemical for that is hydrofloric acid. I found a source but havent got any yet.Exceptionally dangerous stuff, be careful.
https://en.wikipedia.org/wiki/Hydrofluoric_acid#Health_and_safety
https://web.utk.edu/~ehss/training/has.pdf -
I need to etch the scales to get the higher voltage colors and the best chemical for that is hydrofloric acid. I found a source but havent got any yet.
Exceptionally dangerous stuff, be careful.
https://en.wikipedia.org/wiki/Hydrofluoric_acid#Health_and_safety
https://web.utk.edu/~ehss/training/has.pdfOh I know all about it. Killed lots of artists who used it to etch metals. Im only going to use it in the back shed with an exhaust vent. Its sold as rust remover in the US and I can order it from there. Noone in canada sells it.
This stuff is what the other Ti etchers have been using
-
I need to etch the scales to get the higher voltage colors and the best chemical for that is hydrofloric acid. I found a source but havent got any yet.
Exceptionally dangerous stuff, be careful.
https://en.wikipedia.org/wiki/Hydrofluoric_acid#Health_and_safety
https://web.utk.edu/~ehss/training/has.pdfOh I know all about it. Killed lots of artists who used it to etch metals. Im only going to use it in the back shed with an exhaust vent. Its sold as rust remover in the US and I can order it from there. Noone in canada sells it.
This stuff is what the other Ti etchers have been using
What about Multi-Etch? I've seen some YouTubers using it. Not sure what the chemical makeup of it is, but it's supposed to work well for Ti Anodizing.
-
I need to etch the scales to get the higher voltage colors and the best chemical for that is hydrofloric acid. I found a source but havent got any yet.
Exceptionally dangerous stuff, be careful.
https://en.wikipedia.org/wiki/Hydrofluoric_acid#Health_and_safety
https://web.utk.edu/~ehss/training/has.pdfOh I know all about it. Killed lots of artists who used it to etch metals. Im only going to use it in the back shed with an exhaust vent. Its sold as rust remover in the US and I can order it from there. Noone in canada sells it.
This stuff is what the other Ti etchers have been using
What about Multi-Etch? I've seen some YouTubers using it. Not sure what the chemical makeup of it is, but it's supposed to work well for Ti Anodizing.
Bought some but its a pain to work with. Needs to be heated on a hotplate and has a short shelf life when mixed.
-
[quote author=Syph007 link=topic=34772.msg1420061#msg1420061 date=1485837556]
I need to etch the scales to get the higher voltage colors and the best chemical for that is hydrofloric acid. I found a source but havent got any yet.Exceptionally dangerous stuff, be careful.
https://en.wikipedia.org/wiki/Hydrofluoric_acid#Health_and_safety
https://web.utk.edu/~ehss/training/has.pdfOh I know all about it. Killed lots of artists who used it to etch metals. Im only going to use it in the back shed with an exhaust vent. Its sold as rust remover in the US and I can order it from there. Noone in canada sells it.
This stuff is what the other Ti etchers have been using
What about Multi-Etch? I've seen some YouTubers using it. Not sure what the chemical makeup of it is, but it's supposed to work well for Ti Anodizing.
Bought some but its a pain to work with. Needs to be heated on a hotplate and has a short shelf life when mixed.
[/quote]Good to know.
Stay safe if you go the Hydrofluoric Acid route. I still remember the horror stories my Chemistry teachers used to tell about labs that used it... :ahhh
-
I need to etch the scales to get the higher voltage colors and the best chemical for that is hydrofloric acid. I found a source but havent got any yet.
Exceptionally dangerous stuff, be careful.
https://en.wikipedia.org/wiki/Hydrofluoric_acid#Health_and_safety
https://web.utk.edu/~ehss/training/has.pdfOh I know all about it. Killed lots of artists who used it to etch metals. Im only going to use it in the back shed with an exhaust vent. Its sold as rust remover in the US and I can order it from there. Noone in canada sells it.
........Be careful Syph
Here's a report about a lab technician in Oz who carked it due to HF poisoning - Some good recommendations about how to handle HF in the report!!
http://www.ab.ust.hk/hseo/tips/ch/ch005.htm -
I need to etch the scales to get the higher voltage colors and the best chemical for that is hydrofloric acid. I found a source but havent got any yet.
Exceptionally dangerous stuff, be careful.
https://en.wikipedia.org/wiki/Hydrofluoric_acid#Health_and_safety
https://web.utk.edu/~ehss/training/has.pdfOh I know all about it. Killed lots of artists who used it to etch metals. Im only going to use it in the back shed with an exhaust vent. Its sold as rust remover in the US and I can order it from there. Noone in canada sells it.
........Be careful Syph
Here's a report about a lab technician in Oz who carked it due to HF poisoning - Some good recommendations about how to handle HF in the report!!
http://www.ab.ust.hk/hseo/tips/ch/ch005.htmYa skin contact is very brutal with HF. That guy should not have been sitting when working and must not have had the shield down far enough. Crappy way to go out.
That whink rust remover is far lower concentration than what they would have been using considering this is a consumer product and people use it indoors. I dont use any chemicals indoors though, all nasty stuff in back yard shed.
-
compact deluxe tinker today. :D




-
Maybe you have already answered this but how do you get around the problem with the liner "indent" as mentioned in this topic by Gareth?. Even if the real problem (overlapping tools) is only applicable when mixing new and old parts the spring is still thicker than the blade without the indent. Doesn't this result in a wiggly blade?
-
@Fortytwo said:
Maybe you have already answered this but how do you get around the problem with the liner "indent" as mentioned in this topic by Gareth?. Even if the real problem (overlapping tools) is only applicable when mixing new and old parts the spring is still thicker than the blade without the indent. Doesn't this result in a wiggly blade?I make 0.015" phosphor bronze washers to fill out the gap.
-
More beautiful work Syph

-
Maybe you have already answered this but how do you get around the problem with the liner "indent" as mentioned in this topic by Gareth?. Even if the real problem (overlapping tools) is only applicable when mixing new and old parts the spring is still thicker than the blade without the indent. Doesn't this result in a wiggly blade?
I make 0.015" phosphor bronze washers to fill out the gap.
Thank you, you are always very helpful!
-
Another beauty!

JR
Hello! It looks like you're interested in this conversation, but you don't have an account yet.
Getting fed up of having to scroll through the same posts each visit? When you register for an account, you'll always come back to exactly where you were before, and choose to be notified of new replies (either via email, or push notification). You'll also be able to save bookmarks and upvote posts to show your appreciation to other community members.