I Recently Converted My Alox Mod to Torx
-
Nice reference for those looking to attempt this mod.

-
Where did you find those torx screws/pivot barrels?
Edit: just read all replies... nvm
-
Thanks Poncho and Aloha007...
:saknight:Sent from my iPhone using Tapatalk
-
Here's an illustration of how the torx and pivot looks like... at least on my mod... as the diameter of the scale pivot holes are just right for the barrels, and there is enough length for the barrel to go through the scale, counterbore wasn't required...

Maybe counterbore would be required for 1/8" barrels?
Sent from my iPhone using Tapatalk
-
Very cool thread

-
@Mechanickal said:
Where did you find those torx screws/pivot barrels?
Edit: just read all replies... nvm
I just don't know whether Steven sells them to anyone who asks? Or mine were just extras lying around...
Sent from my iPhone using Tapatalk
-
-
@jaya_man said:
Here's an illustration of how the torx and pivot looks like... at least on my mod... as the diameter of the scale pivot holes are just right for the barrels, and there is enough length for the barrel to go through the scale, counterbore wasn't required...
Maybe counterbore would be required for 1/8" barrels?
Sent from my iPhone using Tapatalk
Great sketch - shows the arrangement nicely.

A couple of points to add, from my experience of similar mods (using 3mm brass pivots on all three points):- cut the pivots as long as you possibly can. The more of the pivot that sticks into the scale the better. I assembled the knives onto longer plain rod, measured the overall thickess then subracted 2.5mm to get the final pivot length.
- countersink the ends of the pivot barrels if you can too - this allows the pivots to be longer and have more engagement with the scales for better snap.
- Make the countersinks in the scales as shallow as possible - again, to maximise the overlap between the pivot and the scale.
The screws I used were metric M2x0.5mm with countersunk T6 heads, but I guess the ones Steve used are imperial/standard 2-56.
-
Here's an illustration of how the torx and pivot looks like... at least on my mod... as the diameter of the scale pivot holes are just right for the barrels, and there is enough length for the barrel to go through the scale, counterbore wasn't required...

Maybe counterbore would be required for 1/8" barrels?
Sent from my iPhone using Tapatalk
Great sketch - shows the arrangement nicely.

A couple of points to add, from my experience of similar mods (using 3mm brass pivots on all three points):- cut the pivots as long as you possibly can. The more of the pivot that sticks into the scale the better. I assembled the knives onto longer plain rod, measured the overall thickess then subracted 2.5mm to get the final pivot length.
- countersink the ends of the pivot barrels if you can too - this allows the pivots to be longer and have more engagement with the scales for better snap.
- Make the countersinks in the scales as shallow as possible - again, to maximise the overlap between the pivot and the scale.
The screws I used were metric M2x0.5mm with countersunk T6 heads, but I guess the ones Steve used are imperial/standard 2-56.
Ahhh... more helpful tips for me... I will need it for future mods...
Thanks H :saknight:

Sent from my iPhone using Tapatalk
-
Great thread, and very useful

Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

-
@50ft-trad said:
Great thread, and very useful
Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

Good point... That could be the case too... I suspected that initially... I used the same type of brass pins for my other mods, and I never had to re-peen...
The brass pin material available locally could also be different from those available overseas... The ones I have are actually brass welding rods... I once tried brass pins made in Germany... they were tougher to cut...
Sent from my iPhone using Tapatalk
-
@50ft-trad said:
Great thread, and very useful

Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

Good point... That could be the case too... I suspected that initially... I used the same type of brass pins for my other mods, and I never had to re-peen...
The brass pin material available locally could also be different from those available overseas... The ones I have are actually brass welding rods... I once tried brass pins made in Germany... they were tougher to cut...
Sent from my iPhone using Tapatalk
I meant to talk about brass head forming practices and what Ive learned and this reminded me. In most of the tutorials people show to form the head on one end first then assemble. DONT! Put the pins in unformed and trim to length then peen both heads so they form into the space available. Think about how the space you want to fill is like a countersunk V shape and forming a mushroom head to fit that is not the best fit, and one reason rivets made this way will loosen.
I peen all my 91mm mods this way now so the brass forms nicely into the bushings. It just takes a few taps on one end at a time, and if you have too much brass, file or grind as you work.

-
@50ft-trad said:
Great thread, and very useful

Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

Good point... That could be the case too... I suspected that initially... I used the same type of brass pins for my other mods, and I never had to re-peen...
The brass pin material available locally could also be different from those available overseas... The ones I have are actually brass welding rods... I once tried brass pins made in Germany... they were tougher to cut...
Sent from my iPhone using Tapatalk
I meant to talk about brass head forming practices and what Ive learned and this reminded me. In most of the tutorials people show to form the head on one end first then assemble. DONT! Put the pins in unformed and trim to length then peen both heads so they form into the space available. Think about how the space you want to fill is like a countersunk V shape and forming a mushroom head to fit that is not the best fit, and one reason rivets made this way will loosen.
I peen all my 91mm mods this way now so the brass forms nicely into the bushings. It just takes a few taps on one end at a time, and if you have too much brass, file or grind as you work.

I discovered that if you hit the Brass rod head on just right, repeatedly, the end sort of "bulges" out, increasing in diameter slightly. I think that combined with a nicely formed head, the "bulge" helps fill the brushing?
I hear what you say about not preening until the rod is in the SAK, but I can preen my best when the rod is spinning on a drill.

-
@Pablo O'Brien said:
@50ft-trad said:
Great thread, and very useful

Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

Good point... That could be the case too... I suspected that initially... I used the same type of brass pins for my other mods, and I never had to re-peen...
The brass pin material available locally could also be different from those available overseas... The ones I have are actually brass welding rods... I once tried brass pins made in Germany... they were tougher to cut...
Sent from my iPhone using Tapatalk
I meant to talk about brass head forming practices and what Ive learned and this reminded me. In most of the tutorials people show to form the head on one end first then assemble. DONT! Put the pins in unformed and trim to length then peen both heads so they form into the space available. Think about how the space you want to fill is like a countersunk V shape and forming a mushroom head to fit that is not the best fit, and one reason rivets made this way will loosen.
I peen all my 91mm mods this way now so the brass forms nicely into the bushings. It just takes a few taps on one end at a time, and if you have too much brass, file or grind as you work.

I discovered that if you hit the Brass rod head on just right, repeatedly, the end sort of "bulges" out, increasing in diameter slightly. I think that combined with a nicely formed head, the "bulge" helps fill the brushing?
I hear what you say about not preening until the rod is in the SAK, but I can preen my best when the rod is spinning on a drill.

Interesting... my firsts few mods were peened they way Robert explained... It was challenging for me... a few bent pins in the process... And then I found this impact drill trick... convenient... of course it still needed a few taps here and there so that the pin head will fit nicely into the 91mm bushings... not aesthetically pleasing though... but then celidor scales will hide the ugly peen job... of course exposed pins are a different story... would have to be careful with metal scales...
Sent from my iPhone using Tapatalk
-
@Pablo O'Brien said:
[quote author=50ft-trad link=topic=73215.msg1527672#msg1527672 date=1501430387]
Great thread, and very useful
Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

Good point... That could be the case too... I suspected that initially... I used the same type of brass pins for my other mods, and I never had to re-peen...
The brass pin material available locally could also be different from those available overseas... The ones I have are actually brass welding rods... I once tried brass pins made in Germany... they were tougher to cut...
Sent from my iPhone using Tapatalk
I meant to talk about brass head forming practices and what Ive learned and this reminded me. In most of the tutorials people show to form the head on one end first then assemble. DONT! Put the pins in unformed and trim to length then peen both heads so they form into the space available. Think about how the space you want to fill is like a countersunk V shape and forming a mushroom head to fit that is not the best fit, and one reason rivets made this way will loosen.
I peen all my 91mm mods this way now so the brass forms nicely into the bushings. It just takes a few taps on one end at a time, and if you have too much brass, file or grind as you work.

I discovered that if you hit the Brass rod head on just right, repeatedly, the end sort of "bulges" out, increasing in diameter slightly. I think that combined with a nicely formed head, the "bulge" helps fill the brushing?
I hear what you say about not preening until the rod is in the SAK, but I can preen my best when the rod is spinning on a drill.

Interesting... my firsts few mods were peened they way Robert explained... It was challenging for me... a few bent pins in the process... And then I found this impact drill trick... convenient... of course it still needed a few taps here and there so that the pin head will fit nicely into the 91mm bushings... not aesthetically pleasing though... but then celidor scales will hide the ugly peen job... of course exposed pins are a different story... would have to be careful with metal scales...
Sent from my iPhone using Tapatalk
[/quote]I dont have the patience to peen exposed pins. Cellidor is nice, peen to get the right tension on the rivet, then remove any excess brass stock.
-
Patience is one thing I still need to develop... Good thing there are torx screws and pivots...

Sent from my iPhone using Tapatalk
-
I asked for it, didn't I?

-
@Pablo O'Brien said:
I asked for it, didn't I?
You can't help yourself this morning can you P? :D
Hello! It looks like you're interested in this conversation, but you don't have an account yet.
Getting fed up of having to scroll through the same posts each visit? When you register for an account, you'll always come back to exactly where you were before, and choose to be notified of new replies (either via email, or push notification). You'll also be able to save bookmarks and upvote posts to show your appreciation to other community members.
With your input, this post could be even better 💗
Register Login