I Recently Converted My Alox Mod to Torx
-
@50ft-trad said:
Great thread, and very useful
Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

Good point... That could be the case too... I suspected that initially... I used the same type of brass pins for my other mods, and I never had to re-peen...
The brass pin material available locally could also be different from those available overseas... The ones I have are actually brass welding rods... I once tried brass pins made in Germany... they were tougher to cut...
Sent from my iPhone using Tapatalk
-
@50ft-trad said:
Great thread, and very useful

Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

Good point... That could be the case too... I suspected that initially... I used the same type of brass pins for my other mods, and I never had to re-peen...
The brass pin material available locally could also be different from those available overseas... The ones I have are actually brass welding rods... I once tried brass pins made in Germany... they were tougher to cut...
Sent from my iPhone using Tapatalk
I meant to talk about brass head forming practices and what Ive learned and this reminded me. In most of the tutorials people show to form the head on one end first then assemble. DONT! Put the pins in unformed and trim to length then peen both heads so they form into the space available. Think about how the space you want to fill is like a countersunk V shape and forming a mushroom head to fit that is not the best fit, and one reason rivets made this way will loosen.
I peen all my 91mm mods this way now so the brass forms nicely into the bushings. It just takes a few taps on one end at a time, and if you have too much brass, file or grind as you work.

-
@50ft-trad said:
Great thread, and very useful

Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

Good point... That could be the case too... I suspected that initially... I used the same type of brass pins for my other mods, and I never had to re-peen...
The brass pin material available locally could also be different from those available overseas... The ones I have are actually brass welding rods... I once tried brass pins made in Germany... they were tougher to cut...
Sent from my iPhone using Tapatalk
I meant to talk about brass head forming practices and what Ive learned and this reminded me. In most of the tutorials people show to form the head on one end first then assemble. DONT! Put the pins in unformed and trim to length then peen both heads so they form into the space available. Think about how the space you want to fill is like a countersunk V shape and forming a mushroom head to fit that is not the best fit, and one reason rivets made this way will loosen.
I peen all my 91mm mods this way now so the brass forms nicely into the bushings. It just takes a few taps on one end at a time, and if you have too much brass, file or grind as you work.

I discovered that if you hit the Brass rod head on just right, repeatedly, the end sort of "bulges" out, increasing in diameter slightly. I think that combined with a nicely formed head, the "bulge" helps fill the brushing?
I hear what you say about not preening until the rod is in the SAK, but I can preen my best when the rod is spinning on a drill.

-
@Pablo O'Brien said:
@50ft-trad said:
Great thread, and very useful

Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

Good point... That could be the case too... I suspected that initially... I used the same type of brass pins for my other mods, and I never had to re-peen...
The brass pin material available locally could also be different from those available overseas... The ones I have are actually brass welding rods... I once tried brass pins made in Germany... they were tougher to cut...
Sent from my iPhone using Tapatalk
I meant to talk about brass head forming practices and what Ive learned and this reminded me. In most of the tutorials people show to form the head on one end first then assemble. DONT! Put the pins in unformed and trim to length then peen both heads so they form into the space available. Think about how the space you want to fill is like a countersunk V shape and forming a mushroom head to fit that is not the best fit, and one reason rivets made this way will loosen.
I peen all my 91mm mods this way now so the brass forms nicely into the bushings. It just takes a few taps on one end at a time, and if you have too much brass, file or grind as you work.

I discovered that if you hit the Brass rod head on just right, repeatedly, the end sort of "bulges" out, increasing in diameter slightly. I think that combined with a nicely formed head, the "bulge" helps fill the brushing?
I hear what you say about not preening until the rod is in the SAK, but I can preen my best when the rod is spinning on a drill.

Interesting... my firsts few mods were peened they way Robert explained... It was challenging for me... a few bent pins in the process... And then I found this impact drill trick... convenient... of course it still needed a few taps here and there so that the pin head will fit nicely into the 91mm bushings... not aesthetically pleasing though... but then celidor scales will hide the ugly peen job... of course exposed pins are a different story... would have to be careful with metal scales...
Sent from my iPhone using Tapatalk
-
@Pablo O'Brien said:
[quote author=50ft-trad link=topic=73215.msg1527672#msg1527672 date=1501430387]
Great thread, and very useful
Going back to the original motivation for a moment though, are we sure that it's the brass that's not up to the job. If the pins need repeening, they may be stretching, OR the peened heads may just be "settling" in the holes. I had this happen on one of my mods - everything was tight, but it became a little sloppy with gaps between layers without doing much work. The pins weren't stretching, but the peened heads were pulling in slightly. It may have been that when I was peening, the knife was adequately supported but not the pin itself, and this may have floated slightly when peening the second side.
Hopefully that makes sense

Good point... That could be the case too... I suspected that initially... I used the same type of brass pins for my other mods, and I never had to re-peen...
The brass pin material available locally could also be different from those available overseas... The ones I have are actually brass welding rods... I once tried brass pins made in Germany... they were tougher to cut...
Sent from my iPhone using Tapatalk
I meant to talk about brass head forming practices and what Ive learned and this reminded me. In most of the tutorials people show to form the head on one end first then assemble. DONT! Put the pins in unformed and trim to length then peen both heads so they form into the space available. Think about how the space you want to fill is like a countersunk V shape and forming a mushroom head to fit that is not the best fit, and one reason rivets made this way will loosen.
I peen all my 91mm mods this way now so the brass forms nicely into the bushings. It just takes a few taps on one end at a time, and if you have too much brass, file or grind as you work.

I discovered that if you hit the Brass rod head on just right, repeatedly, the end sort of "bulges" out, increasing in diameter slightly. I think that combined with a nicely formed head, the "bulge" helps fill the brushing?
I hear what you say about not preening until the rod is in the SAK, but I can preen my best when the rod is spinning on a drill.

Interesting... my firsts few mods were peened they way Robert explained... It was challenging for me... a few bent pins in the process... And then I found this impact drill trick... convenient... of course it still needed a few taps here and there so that the pin head will fit nicely into the 91mm bushings... not aesthetically pleasing though... but then celidor scales will hide the ugly peen job... of course exposed pins are a different story... would have to be careful with metal scales...
Sent from my iPhone using Tapatalk
[/quote]I dont have the patience to peen exposed pins. Cellidor is nice, peen to get the right tension on the rivet, then remove any excess brass stock.
-
Patience is one thing I still need to develop... Good thing there are torx screws and pivots...

Sent from my iPhone using Tapatalk
-
I asked for it, didn't I?

-
@Pablo O'Brien said:
I asked for it, didn't I?
You can't help yourself this morning can you P? :D
-
Getting peened heads to look good is a practice thing. Lots of it.
Also the torx pivots were made by someone else with a cnc machine and not anyone here. The "brass" pivots are not brass but a special copper that was heat treated. They were made specifically for me to my specs. As Syph can tell you quality matters when it comes to pivots.
Btw, I'm still around and lurk in the shadows always watching. -
Hey Steven, nice to know your still around... Guess you know the next question some will be asking... Can we still get some? :lol:
Sent from my iPhone using Tapatalk
-
Steve,
Do you remember the actual specs of the "special copper" matwrial that you used.
I'm considering getting some pivots made as l can't make myself pay close to $100 to order a handful of pivots from Alpha Knife Supplies ($ 50 min order plus international postage plus the exchange rate).
Cheers
George -
Would the 1/8" ones not be easy to convert to 3mm by screwing them onto a hex head bolt held in a drill chuck, spinning it up and sanding down a little on a bit of emery? There's very little between the two sizes, so I wouldn't have thought that the wall thickness reduction would be detrimental
-
The 1/8" pivots are hardened stainless.
-
The pivots were part of a deal I had with Tattoosteve99... An awesome guy and friend... A good person to deal with...
Sent from my iPhone using Tapatalk
First of all, great mod!!

As george1 said,@george1 said:
"...I've been holding off on buying the 1/8" pivots from the recommended place as they have a $US 50 minimum order (not including postage) for overseas buyers..."I've also been searching everywhere for just the right size pivots, but no luck so far... until now!! This is maybe great news... if stock still exists
@tattoosteve99 said:
Getting peened heads to look good is a practice thing. Lots of it.
Also the torx pivots were made by someone else with a cnc machine and not anyone here. The "brass" pivots are not brass but a special copper that was heat treated. They were made specifically for me to my specs. As Syph can tell you quality matters when it comes to pivots.
Btw, I'm still around and lurk in the shadows always watching.Are there any pivots left?
I'd gladly take a set of them off your hands. I'll shoot you a PM. -
What was the length of the pivots used for this mod?
It seems that the longest 1/8" pivot that are available are 0.5" and the longest 3.0mm tap that l can find is about 14 mm.
I'm now thinking that if l get some 3.0mm pivots made, the tapped hole wont go all the way through. -
The pivot barrels are 0.5" in length...
Sent from my iPhone using Tapatalk
Hello! It looks like you're interested in this conversation, but you don't have an account yet.
Getting fed up of having to scroll through the same posts each visit? When you register for an account, you'll always come back to exactly where you were before, and choose to be notified of new replies (either via email, or push notification). You'll also be able to save bookmarks and upvote posts to show your appreciation to other community members.